标准 | GB12771-2000 | HG20537.2-92 | HG20537.3-92 | HG20537.4-92 | ASTM A312/A312M | ASTM A249/A249M | ASTM A688/A688M | JISG3468 | |||||||||||||||
项目 | |||||||||||||||||||||||
牌号 | 0Cr19Ni9
00Cr19Ni10 0Cr17Ni12Mo2 00Cr17Ni14Mo2 0Cr18Ni10Ti (1Cr18Ni9Ti) |
0Cr18Ni9
00Cr19Ni10 0Cr17Ni12Mo2 00Cr17Ni14Mo2 0Cr18Ni10Ti (1Cr18Ni9Ti) |
0Cr18Ni9
00Cr19Ni10 0Cr17Ni12Mo2 00Cr17Ni14Mo2 0Cr18Ni10Ti (1Cr18Ni9Ti) |
0Cr18Ni9
00Cr19Ni10 0Cr17Ni12Mo2 00Cr17Ni14Mo2 0Cr18Ni10Ti (1Cr18Ni9Ti) |
TP304 TP304L
TP316 TP316L TP321 |
TP304 TP304L
TP316 TP316L TP321 |
TP304 TP304L TP304N
TP316 TP316N TP316L TP304LN TP316LN |
SUS304TPY
SUS304LTPY SUS316TPY SUS316LTPY SUS321TPY |
|||||||||||||||
规格范围(mm) | D<=630 | 10<=D<=76 | D<=325 | 377<=D<=1020 | 10.3<=D<=762 | D<=127 0.4<=t<=8.1 | 15.9<d<=25.4 75<=D<=1200或更大t>=0.7 | 165.2<=D<=1016 | |||||||||||||||
屈服强度ó0.2(Mpa) | >=180;>=210 | >=175;>=205 | >=175;>=205 | >=175;>=205 | <=170;>=205 | >=170;>=215 | >=175;>=205;>=240 | >=175;>=205 | |||||||||||||||
抗拉强度ób(Mpa) | >=480;>=520 | >=480;>=520 | >=480;>=520 | >=480;>=520 | >=485;>=515 | >=485;>=515 | >=485;>=515;>=550 | >=480;>=520 | |||||||||||||||
延伸率§5(%) | >=35(焊态>=25) | >=40 | >=40 | >=40 | >=35 | >=35 | >=35 | >=35(横向>=25) | |||||||||||||||
焊缝横向弯曲或展平 | 展平 t;=200弦高H=D/4 | 反向展平 | - | 正弯、反弯、弯芯直径d=3t | 焊缝横向导面弯曲ASTM370 | 反向弯曲(d=4t)或展平 | 同左 | 特殊要求JISZ3122 | |||||||||||||||
压扁试验(mm) | D<200 H=D/3 | H=1.09t/(0.09+t/D) | H=1.09t/(0.09+t/D) | - | - | H=1.09t/(0.09+t/D)并试验完好性 | - | - | |||||||||||||||
扩口、卷边 | - | a=60° 扩20%D | - | - | - | 卷边宽度15%D | 卷边宽度15%D | - | |||||||||||||||
无损探伤 | - | GB/T7735 B级 | GB/T 7735 A级当t>6.3mm时应达到GB3323III级(20%) | GB3323 100%x射线II级
20%x射线III级 |
补充要求(射线探伤) | 代替水压 | 补充要求(涡流探伤) | 特殊要求JISZ3106 | |||||||||||||||
压力试验(Mpa) | 水压 | Pmax=10可用涡流探伤代替GB/T7735A级 | 双方协议可用无损探伤代替
P=2Rt/D 式中R=50% ó0.2Pmax=7.5 |
1.5-6.0按壁厚系列分或经双方协议用无损探伤代替Pmax=2Rt/D式中R=50%ó0.2 | 1.5-2.5按壁厚系列分或经双方协议用缝缝探伤代替 | ASTM A530/A530M
D<=270 P=2Rt/D式中R=50%ó0.2 |
可用无损探伤代替 | ASTM A450/A450M | 1.5-2.5按壁厚系列分 | ||||||||||||||
气压 | - | P=1MPa | |||||||||||||||||||||
晶腐试验 | GB4334.5 | 附加要求GB4334.5 | 附加要求GB4334.5 | 附加要求GB4334.5 | ASTM A262E法(补充要求) | ASTM A262E法(补充要求) | ASTM A262E法(补充要求) | - | |||||||||||||||
热处理 | 要求 | 要求 | 要求 | 附加要求 | 要求 | 要求 | 要求 | 特殊要求 | |||||||||||||||
I级 | II级 | ||||||||||||||||||||||
外径偏差(mm) | 焊
态 |
外径 | 普通 | 高级 | 外径 | 允许偏差 | 外径 | 允许偏差 | 外径 | 允许偏差 | ±1%D(D按周长测算) | 外径 | 允许偏差 | 外径 | 允许偏差 | 外径 | 允许偏差 | 外径 | 允许偏差 | ||||
<20 | ±0.30 | ±0.20 | <25 | ±0.10 | <=10 | ±0.15 | <=168 | ±0.75%D最小值为±0.3 | 10.3-48.3 | +0.40/-0.80 | <25.4 | ±0.10 | <25.4 | ±0.10 | <=318.5 | ±1%D | |||||||
>=20-<50 | ±0.50 | ±0.40 | 25-38 | ±0.15 | >10-30 | ±0.20 | >48.3-114.3 | +0.80/-0.80 | 25.4~<=38.1 | ±0.15 | 25.4~<=38.1 | ±0.15 | - | - | |||||||||
>=50 | ±1%D | ±0.80%D | >38-<51 | ±0.20 | >30-50 | ±0.30 | >114.3-219.1 | +1.60/-0.80 | >38.1~<50.8 | ±0.20 | >38.1~<50.8 | ±0.20 | - | - | |||||||||
固溶态 | <13 | ±0.25 | ±0.20 | 51-63 | ±0.25 | >50 | ±0.8%D | >219.1-457.2 | +2.40/-0.80 | 50.8~<63.5 | ±0.25 | 50.8~<63.5 | ±0.25 | - | - | ||||||||
>=13-<25 | ±0.40 | ±0.30 | >=63-76 | ±0.30 | - | - | >457.2-660.4 | +3.20/-0.80 | 63.5~<76.2 | ±0.30 | 63.5~<76.2 | ±0.30 | >318.5 | ±0.5%D | |||||||||
>=25-<40 | ±0.60 | ±0.40 | - | >168-325 | ±1%D | >660.4-864 | +4.00/-0.80 | 76.2~<=101.6 | ±0.38 | 76.2~<=101.6 | ±0.38 | - | - | ||||||||||
>=40-<65 | ±0.80 | ±0.60 | >864-1219.2 | +4.80/-0.80 | >101.6~<=190.5 | +0.38/-0.64 | >101.6~<=190.5 | +0.38/-0.64 | - | - | |||||||||||||
>=65-<90 | ±1.00 | ±0.80 | - | >190.5~<=228.6 | +0.38-1.14 | >190.5~<=228.6 | +0.38-1.14 | - | - | ||||||||||||||
>=90-<140 | ±1.20 | ±1.00 | - | - | - | - | - | - | |||||||||||||||
>=140-<300 | ±1.5%D | ±1.0%D | - | - | - | - | - | - | |||||||||||||||
>=300-<500 | ±1.0%D | ±0.8%D | - | - | - | - | - | - | |||||||||||||||
>=500 | 按协议 | 按协议 | - | - | - | - | - | - | |||||||||||||||
壁厚偏差(mm) | 壁厚 | 允许偏差 | ±0.10%t,最小允许偏差为±0.2,可双方协议为+18%t/D | ±0.10%t,最小允许偏差为±0.2 | D<=508 | t<=8 | +15%t/-12.5%t | ±不规定/-12.5%t | ±10%t | 平均壁厚允许偏差±10%t
最小壁厚允许偏差±20%/D |
D<=508 | t<8 | +15%t/-12.5%t | ||||||||||
t>8 | +15%t/-10%t | ||||||||||||||||||||||
<=4 | ±0.5/-0.6 | t;508 | t<=8 | +不定%t/-12.5%t | t>=8 | +15%t/-10%t | |||||||||||||||||
>4 | ±10%S | t>8 | +不定%t/-10%t | t;=558.8 | t<8 | +不定%t/-12.5%t | |||||||||||||||||
t>=8 | +不定%t/-10%t | ||||||||||||||||||||||
不圆度偏差 | - | 同外径偏差 | 同外径偏差 | <=1.5%D | <=1.5%D | - | - | - | |||||||||||||||
弯曲度(mm/m) | 2.0mm/m~2.5mm/m | 1.0mm/m | 3.0mm/3m | 5mm/3m | 合理的直度 | 0.8mm/900mm | - | 实用性平直 | |||||||||||||||
焊缝余高(mm) | 最大不超过1.5mm | 外缝余高与母材平
内缝余高D<20 <=0.15; t;=20 <=0.25 |
外缝余高与母材平
内缝余高<=15%t |
内缝余高<=25%t且<=3
外缝余高<=50%t且<=3 |
- | - | - | 特殊要求内缝余高<=1.5
外缝余高<=3.0 |
|||||||||||||||
其他要求 | - | HRB<90 | - | - | HRB<=90 | HRB<=90 | HRB<=90 | - |
ASTM不锈钢标准—钢管
ASTM A213 无缝铁素体和奥氏体合金钢锅炉、过热器和换热器管
ASTM A249 锅炉、过热器、换热器和冷凝器用焊接奥氏体钢管
ASTM A268/A268M-10 一般用铁素体和马氏体不锈钢无缝和焊接钢管
ASTM A269 -10 一般用途无缝和焊接奥氏体不锈钢管
ASTM A270/A270M-10 卫生设备用无缝和焊接奥氏体不锈钢
ASTM A312/A312M-09 无缝、焊接和冷加工用奥氏体不锈钢管
ASTM A358 高温用电熔焊奥氏体铬镍合金钢管
ASTM A381 高压输送用金属弧焊钢管
ASTM A409 腐蚀场所或高温下使用的焊接大口径奥氏体钢管
ASTM A688/A688M-10 给水加热器用奥氏体不锈钢焊管
ASTM A733-03(2009)e1 碳素钢和奥氏体不锈钢焊接和无缝螺纹钢管
ASTM A778 焊接未退火的奥氏体不锈钢管形制品
ASTM A789/A789M-10 一般用途无缝和焊接铁素体/奥氏体不锈钢管
ASTM A790/A790M-09a 无缝与焊接铁素体/奥氏体不锈钢管
ASTM A791 不退火铁素体焊接不锈钢管
ASTM A803 焊接铁素体不锈钢给水加热器管
ASTM A813 单或双焊接奥氏体不锈钢管
ASTM A814/A814M-08 冷加工焊接奥氏体不锈钢管
ASTM A826/A826M-95 增殖反应堆堆芯部件用奥氏体和铁素体不锈钢管
ASTM A872/A872M-07a 腐蚀环境下用离心铸造铁素体/奥氏体不锈钢管
ASTM A928/A928M-09a 填充金属电熔焊铁素体/奥氏体不锈钢管
ASTM A999/A999M-04a(2009) 合金钢及不锈钢管一般要求
ASTM A1016/A1016M -08 铁素体和奥氏体不锈钢管的一般要求
结构用不锈钢管
ASTM A511/A511M-08 机械工程用不锈钢无缝管
ASTM A554 焊接不锈钢机械管(圆形,方矩形,椭圆型)
ASTM A632-04(2009) 一般设备用无缝和焊接奥氏体不锈钢管(小直径)
ASTM A908 不锈钢针管
材质:304,304L,316,316L,409D,321,2205,2507,S31803.